Talk Composites - The Forum for Advanced Composites

Very high temp epoxy resin

http://www.talkcomposites.com/Topic19870.aspx

By alex.mc - 11/18/2015 9:30:08 AM

Question,

Can the High temp resin be used in a "hot tool" process?

What I mean is, can the cure be accelerated by elevating the temperature during cure? I suspect it will increase of course, and I understand a post cure is not the same thing, but I am wondering if stable metal moulds could be used with this resin to produce a quick turn around time?

I looked at the data sheets, but could not find a list of curing times against the ambient temp.