What is the best way to soften the glue on the back of pro finish fabric?
As I've got a complex shape which is tricky to get the fabric to lay down in to.

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You can heat it a bit with a heat gun but it just isn't great for complex parts. 
Darren
Darren
Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)
Group: Forum Members
Posts: 54, Visits: 916
What about misting the back of regular twill with a spray tack? Just to hold it slightly.

I have aerofix 2..

The reason i ask is because i want to lay up with two pieces of fabric instead of one.
I made it with one piece in the pic below but is messy around the top


Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yep, I prefer that to using set-weave fabrics. Gives you the same stability, but I find you can still massage it into place for a time (after too long the adhesive becomes a bit too solid and the fabric handles a bit more like a standard set-weave). 
Darren
Darren
Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)
Group: Forum Members
Posts: 54, Visits: 916
Ok cool i shall try that Smile