Hello all, I have joined to gain knowledge on vacuum bagging. I have had one attempt making a mould and a few leaks occurred which set the cat among the birds to coin a saying and in the end in went to the bin.
I was making a rear defuser for F3 race car, apart from the leaks in the mould I used foam as a stiffner to make the ribs under the defuser and when vacuum was pulled it deformed the foam and problems after that, so that's where I am at the moment.
I have made another mould and would appreciate some body that has made these before that could make a few suggestion.
Please understand that I have little knowledge in vacuum bagging however used heaps of glass and fiber in hand lay up's