thanasiss3
thanasiss3
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 18,
Visits: 348
Hi everyone,i skin parts for automotive interiors with cf using the ec high temp epoxy resin,after the wrapping i wet the fabric with epoxy,after 24hours i sand with 120grit and after that add 2 layers of epoxy when the first is at tack free stage.
After that i put the parts in an oven and ramp the temp at 100celcius,after that i have too much amine blush,it can stick to my hand,is this normal?
Is there any chance the epoxy to keep blushing under the 2k clearcoat and give me a yellowish pary?
I must wait more time to cure after the complete cycle at the oven?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Skinning amine blush
thanasiss3
-
10 Years Ago
Sounds a bit strange to me ... I have never had Amine blush problems with the High-temp resin -- ???...
Dravis
-
10 Years Ago
What can cause the 'yellowish' of the carbon skinned glovebox ?this epoxy is easycomposites high...
thanasiss3
-
10 Years Ago
The high temperature resin is not perfectly colourless to begin with. It is a slight pale amber in...
Warren (Staff)
-
10 Years Ago
I agree with Warren in that the ht resin is not water clear. can I ask why you've used it on the...
VVS
-
10 Years Ago
In greece under a hot summer day i measure 85 celcious into the car,it became extremely hot and the...
thanasiss3
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search