Sounds a bit strange to me ... I have never had Amine blush problems with the High-temp resin -- ??? But it does take a very long time to cure completely .. I have only used high temp for skinning once, and had no problems. It was cured at 50 -60 deg. C. for 24 hours + a bit -- Then postcured at 100 for 2 hours, just to raise the Tg a bit.. (Non critical part)