fastboats
fastboats
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 9,
Visits: 94
Looking to make a mold of a small performance boat hull.
I have read that in order to make a very good mold that will last a long time some use carbon fiber vs fiberglass mat in a unimold type setup.
Once the part is setup and flanges in place can I apply gel wait for that to tack and apply a layor of carbon down and expoy coat over that?
Or will the Gel delaminate from the mold?
Thanks for any help and please go easy I'm new and learning as much as I can.
Edited
11 Years Ago by
fastboats
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Gel coat and Epoxy if done correctly will it work?
fastboats
-
11 Years Ago
you use carbon same as glass fibers. in poly resin watch for wax contamination on surface, it...
wojtepanik
-
11 Years Ago
Are you talking about "mixing" Unimould Gel-coat with epoxy for backing?? That will probably not...
Dravis
-
11 Years Ago
I'm not certain that it wouldn't work... I've used epoxy tooling gelcoat and backed it up with vinyl...
Hanaldo
-
11 Years Ago
Yes, but I think that has to do with what will bond to what, and in which "state" Both Polyester...
Dravis
-
11 Years Ago
Yeh that is my one doubt... But I'm not so sure that wax additive would be a bad solution. Once...
Hanaldo
-
11 Years Ago
OK I found GC50 clear but I want black can I add color somehow? Add a pigment or spray clear and...
fastboats
-
11 Years Ago
Edited.
fastboats
-
11 Years Ago
sorry to thread jack, but if im reading this right. You can use epoxy gelcoat and follow up with VE...
kidpaint
-
11 Years Ago
Correct. Just watch for styrene attack. If the epoxy isn't sufficiently cured, the styrene can...
Hanaldo
-
11 Years Ago
I am curious why the original poster want to use epoxy resins. I have not used the specific Uni...
Fasta
-
11 Years Ago
So I could get some gc50 color it as I want then apply to a surface (mold release applied first)...
fastboats
-
11 Years Ago
In my experience the first and main thing that makes or defines the mould is the surface quality...
Fasta
-
11 Years Ago
OK I'm sorry I missed a post. I'm looking to make a long lasting mold. I was reading that the non...
fastboats
-
11 Years Ago
The uni mold like many others is a no shrink system. It should be good. (note I have not...
Fasta
-
11 Years Ago
I understand what your saying for the most part. And thanks for the information. One thing I don't...
fastboats
-
11 Years Ago
Because it's not good practice to lay all your reinforcement in one hit, like you can do with rapid...
Hanaldo
-
11 Years Ago
OK so the heat generated would be the problem with more then a few layers of epoxy on a half layup...
fastboats
-
11 Years Ago
OK I searched the csm and now understand it the binding agent that causes problems with epoxy.
fastboats
-
11 Years Ago
Using epoxy wont create excessive heat with just 4-5mm thick. Using CSM builds thick laminates...
Fasta
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search