Equipment for applying gelcoat


Author
Message
67redrocket
67redrocket
Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)
Group: Forum Members
Posts: 49, Visits: 486
I see that the GC50 is used before laying up the carbon on high gloss parts. But what do you use to apply it? I think the easy composites gelcoat spraying cup gun is a bit expensive, is there other ways to apply it and still get a high gloss result? Can for example a plastic spray bottle be used?

For those that use the spray cup gun, how do you clean it after use?
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search