How do i prepare existing Cf surface for bonding with new prepreg ?
How do i prepare existing Cf surface for bonding with new prepreg ?
Post Reply
Like
3
How do i prepare existing Cf surface for bonding with new prepreg ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
creator
creator
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 9,
Visits: 92
Hello ,
If i want to make a repair in an existing Carbon Fiber structure using prepreg material how do i preprer
the existing surface ?
1) Remove all th upper layer of paint or whatever showing the carbon fiber
2) Clean the surface with what ????
Water ???
Airblow ???
A new piece of cloth??
Easy Leasy mould cleaner ?????
3) And then Just lay on top the prepreg ??
Reply
Like
3
Fasta
Fasta
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
I usually just blow the dust off and carry on with the next layers of pre preg.
Sure you could also clean it with acetone, iso alcohol or other too but I don't think clean ground epoxy surface will be of any concern?
Fastacraft Facebook page
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search