Yeah that's all i being doing reading the pdf and watching the movie.
Guess i gotta order some more regular weave, and don't cut it off until i got 1 layer of top coat on.

Because what is being done in the video definitely does not work for me.
My weave gets all messed up when i trim it.
Warren
Warren
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Administrators
Posts: 214, Visits: 782
You could use profinish on the flatish pieces for perfectly straight weave, but you shouldnt need to on such pieces.

read this instruction manual for skinning:
Instructions

And watch this video:


Should answer most of your questions in far more detail than words can easily describe.
YvesT
YvesT
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 6, Visits: 20
When exactly is the right time to trim the pieces?
After you let the firs top layer cure for a night?
Or when you put the last top layer on and have that cured?

If i look at how some people have a big piece of fabric on their part i can't understand how everything sticks into place.

Is it about how sticky the base coat is or is there something else.
Since you can't really force it to stay in place with something.

Is he ProFinish frabric even possible to use on parts like i have shown?
Warren
Warren
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Administrators
Posts: 214, Visits: 782
are you trimming the fabric quite close to the edge when you lay it on??  if so use a bigger bit of fabric so the edges hold together during laminating. You can trim the edges once its cured.
YvesT
YvesT
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 6, Visits: 20
These are some pictures from parts id like to get in CF.
As you can see the center console has some parts done already, some which failed big time.
No surprise since i have never done it.
Used the Carbon fiber beginner skinning kit with the regular 2/2 fabric

http://i47.tinypic.com/iqifja.jpg
http://i47.tinypic.com/2sajvpd.jpg
http://i46.tinypic.com/m3f2d.jpg



http://i48.tinypic.com/1zlcaag.jpg
http://i47.tinypic.com/iyfleq.jpg
http://i50.tinypic.com/244u15x.jpg
http://i48.tinypic.com/opn2wx.jpg
http://i47.tinypic.com/a428ee.jpg
http://i48.tinypic.com/fejmtl.jpg
http://i48.tinypic.com/14o4zur.jpg


If i had any options of letting someone do it for me i probably would.
But the few people/companies i found were asking close to 3-4k € doing it.
It's cheaper to buy original parts with CF at that price.

I know with some more practice i can figure it out.
Though i am curious if i would be better of using the ProFinish 2/2 fabric?
I seem to mess things up a lot with the edges, where the fabric is very fragile.
Which in turn gives a bad finish at the edges.
And as  you can see some parts have angles and curves, which will be tricky for the inexperienced person.

From what i can gather the ProFinish makes life a little easier, though the description mentions is mainly used for flat surfaces.

The flat areas are not much of an issue, its the curved and corners which are where i mess things up.
I also might need to be less conservative with the fabric.
Though 1 part the shift knob trim had some weird hazy spots, which i cannot explain.
By the time i sanded them out there was very little left of my top coat.

Any advice would be welcome.
Thanks
Edited 13 Years Ago by Warren