Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Metal inserts - Carbon fiber layup
Metal inserts - Carbon fiber layup
Post Reply
Like
24
Metal inserts - Carbon fiber layup
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Trace Elliott
Trace Elliott
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 30
Hello everyone,
I'm designing a drone, and I would like to be able to bolt two plates together (rather than use an adhesive, because if something breaks, I'd prefer to be able to change the piece that broke, rather than a whole assembly).
The plates would be 2-3mm thick, made by resin infusion.
To that effect (bolting plates together), I'd like to put a metallic insert in the lamination, prior to the infusion.
The insert would be a nut, essentially.
I know you can make the plate, then drill a hole and glue the insert, but I'd rather infuse the whole thing at once, if it's possible.
My question is: how do you put an insert in the fiber stack?
I read everywhere that you should have pins in the mould to accurately locate the inserts, but very little info on how to blend the insert in the fiber stack.
Should I spread the fibers apart? I'm thinking that won't look good
Should I punch a hole through the stack? Hello fibers everywhere...
Should I lay the first cloth and spread the others around the insert, and grind the first layer to reveal the insert?
If you have any ideas, please do tell :-)
Thank you very much!
Reply
Like
24
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Metal inserts - Carbon fiber layup
Trace Elliott
-
11 Years Ago
There is no set way to do it as it varies with design. ideally on a straight forward sheet you would...
Warren (Staff)
-
11 Years Ago
Thanks for the tips, that's really helpful! I understand how to position the insert, what I don't...
Trace Elliott
-
11 Years Ago
I should think the insert I'm the picture is fitted after. the cf would be drilled and then the...
VVS
-
11 Years Ago
I have actually conducted several tests of bonding in and laminating in metal fasteners (made from...
Dravis
-
11 Years Ago
In the past I've scored the surface of some small bits of sheet metal and then put that in the...
FLD
-
11 Years Ago
How thick a piece of metal are you using? I always think of sheet metal as being like 0.5 to 3mm...
Hanaldo
-
11 Years Ago
[quote][b]Hanaldo (13/09/2015)[/b][hr]How thick a piece of metal are you using? I always think of...
FLD
-
11 Years Ago
Well .. thickness of the metal insert with relation to the strength of the fastening depends...
Dravis
-
11 Years Ago
Apart from when ive been laying up prepreg tooling ive never put inserts into the laminate stack....
scottracing
-
11 Years Ago
Post Reply
Like
24
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search