I would have said so, the best thing to do is probably join it at the center of the roof as there will always be a noitceable joint but if it's in the center it won't look bad. If your using a twill weave you could even mirror the weave on the other side of the joint and make the joint a feature so a birds eye view of the carbon weave on the roof instead of looking like this: \\\\\\\ it would look like this: <<<<<<

I think you would have to use some profinish to keep it looking neat.

Dave.
andelise
andelise
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 7, Visits: 81
hi guys im thinking of rapping my hole car in 2/2 twill carbon and give about 10 coats of clear coat.

when it comes to the roof it would need to come down the pillers and rear 1/4 pannel in one

or can it be joined?

if so is it a butt joint lining up the patten like you would wall paper?

any help would be really helpful

thanks all
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search