Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Resign Tacky after 24 hours
Resign Tacky after 24 hours
Post Reply
Like
3
Resign Tacky after 24 hours
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
eastdave2
eastdave2
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 5
Telephone call to the boys on a bank holiday weekend sorted, take the rest of the weekend off Cheers Dave.
Reply
Like
2
eastdave2
eastdave2
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 5
I am covering some exsisting glass fibre RC aircraft legs with light weight carbon, the Epoxy Coating resign mixed two to one has had over 24 hours yet still feels tacky, WHY? rescent ambient temp in 20's
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search