I am covering some exsisting glass fibre RC aircraft legs with light weight carbon, the Epoxy Coating resign mixed two to one has had over 24 hours yet still feels tacky, WHY? rescent ambient temp in 20's
eastdave2
eastdave2
Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)
Group: Forum Members
Posts: 2, Visits: 5
Telephone call to the boys on a bank holiday weekend sorted, take the rest of the weekend off Cheers Dave.Smile