Hi, I'm just working on some structural calcs; does anyone have the material properties for the fibre used in the standard carbon cloth, tensile strength, youngs modulus etc. any info like this would be really appreciated.

Cheers, M
Reply
maggie
maggie
Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)
Group: Forum Members
Posts: 7, Visits: 43
Hi Paul,

            I assume this calculation assumes the TORAY 300 mentioned previously.

I have some additional queries shown below:-

1. What would be the impact of using a stiffer 2x2 TWILL  cloth based upon TENAX UMS 40 or TORAYCA M340J for example ?

2. Can easy composites supply such a clith described in 1

3.  Does your calcutation apply equally to the wet lay up material or PRE-PEG material

4.  What is the difference in properties if the carbon/kevlar 2x2 TWILL material is used?

                                                                                                                                                Cheers,

                                                                                                                                                                  Maggie
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
MAVERICK - 14 Years Ago
Paul (Staff) - 13 Years Ago
H_Brett - 13 Years Ago
Matt (Staff) - 13 Years Ago
Paul (Staff) - 13 Years Ago
maggie - 13 Years Ago
hierlchr - 12 Years Ago
carboncomposite - 12 Years Ago
Warren (Staff) - 12 Years Ago
Warren (Staff) - 12 Years Ago
carboncomposite - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search