Bend Radius


Author
Message
Frankentech
Frankentech
Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)
Group: Forum Members
Posts: 2, Visits: 9
That's great, much appreciated Smile
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Frankentech,

The rods cope well with flex providing that the flex does not exceed the sheer strength of the epoxy (this is normally where they will fail leading to them fracturing, rather than the carbon breaking).

In terms of the minimum bend radius this isn't data that I have specifically for each rod but in a less scientific sense I've just bent a 3mm rod through 90 degrees over a radius of 260mm and the 4mm 90 degrees over 360mm and they returned to their original straightness without any trouble. At those radiuses the rods are pretty hard to bend much further although how far I could have gone before they would have fractured I'm not quite sure.

I hope this helps you.

Best regards, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Frankentech
Frankentech
Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)
Group: Forum Members
Posts: 2, Visits: 9
Hi, I was wondering about what radius the 3mm and 4mm carbon rods can be bent to and how well they cope with flexing