We are trying to create carbon wing (see photos) from textrem with infusion, almost whole wing is ok, but last part, after few minutes on sun it goes wrong.

Can you please give us some hint, what we are doing wrong?

http://www.talkcomposites.com/Uploads/Images/1d26313f-08d3-4bcf-893a-f4e1.jpg
http://www.talkcomposites.com/Uploads/Images/45602c20-0b14-42f2-9d23-44b4.jpg