Hiya,
I recently bought the starter kit, and the web page gives silicone:catalyst ratios as 10:1, while the labels in the products themselves give 100:5. I was wondering which is accurate.

Thanks.
Edited 11 Years Ago by AeronMitchell
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The silicone which comes with the linked starter kit is our CS2 Condensation Cure Silicone Rubber  Which you can use with a catalyst ratio of between 2 and 5% as per the Starter Kit instructions and CS2 datasheet.


I'm not sure where the 10 to 1 has been mentioned but if there is a typo you can see then I would be grateful for a link so i can correct it!


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
AeronMitchell
AeronMitchell
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 2, Visits: 3
The 1:10 was on the page I linked to (before it was changed shortly after I posted this). So it's been sorted out now.http://www.talkcomposites.com/Uploads/Images/a38c509d-0c53-4486-b787-2860.png