By AeronMitchell - 5/29/2015 2:13:11 PM
Hiya, I recently bought the starter kit, and the web page gives silicone:catalyst ratios as 10:1, while the labels in the products themselves give 100:5. I was wondering which is accurate.
Thanks.
|
By AeronMitchell - 5/29/2015 6:22:04 PM
The 1:10 was on the page I linked to (before it was changed shortly after I posted this). So it's been sorted out now.
|
|