k9
k9
k9
posted 11 Years Ago HOT
Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)
Group: Forum Members
Posts: 5, Visits: 31
hi

im loking at the pros and cons of pre preg as it cost more to bye but you don't need to bye the resin so does it work out the same price? obviously ill need to make an oven and vac pump but just wondering how it all works out




so give me your views on pre preg against resin infusion




cheers Rob 