Ronny
Ronny
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 58,
Visits: 401
Hi
Yesterday i really hammered the carbon lip on my front bumper, and it is really annoying.
Now i want to repair this myself, but i hope someone here can help me in the right direction.
If you look at the pictures you can see how the damage is.
Now my plan is to sand the whole lip down with 120grain wet sandpaper untill it seems even.
Then ill use a brush and apply epoxy laminating resin with a brush over the sanded area.
After this ill let the resin harden and then and it down with 800 and 1200 wet sandpaper.
Will this work and can i expect the reults to be pretty good?
Should i use anything to clean of the lip before applying the resin?
Any help appreciated
Attachments
carb.jpg
(
672 views,
71.00 KB
)
carb2.jpg
(
619 views,
99.00 KB
)
Reply
Like
3
scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
depending on how much you have tosand back you might get away with floodcoating of a 2k lacquer, rather than using resin as you will have to sand that back then polish to get a nice finsih
Reply
Like
2
Ronny
Ronny
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 58,
Visits: 401
At some parts i see right through to the carbon fibre, so all the resin is worn off.
This means i have to use resin right?
Reply
Like
3
ChrisR
ChrisR
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
Sand, fill any deep bits with epoxy then lacquer.
It's non structural so don't worry about it too much, the white scars will go once you've sanded and lacquered
Reply
Like
3
Ronny
Ronny
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 58,
Visits: 401
When you say lacquer, what product do you mean?
Could you point me to one type of lacquer product?
In my head the epoxy resin would both fill and once properly sanded and buffet it would get a nice clear surface.
Edited
10 Years Ago by
Ronny
Reply
Like
3
Ronny
Ronny
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 58,
Visits: 401
I just did some research and it is a clear coating i need, for uv protection?
So ill add this to my list aswell, will be appyling the resin tomorrow, fingers crossed.
Reply
Like
3
ChrisR
ChrisR
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
Yup, its for UV protection and also allows you to control the finish a bit more, gloss/satin etc...
For your project, rattle can lacquer from Halfords or similar car part store would suffice
http://www.halfords.com/motoring-travel/cleaning-body-repair/car-spray-paints/halfords-clear-lacquer-500ml
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search