Hi guy 

Bought some fibre 2/2 twill 3k,  and the el2 slow epoxy,  I will be using glass to make the sheet on, I would like the size to be 400mm x 300mm 

So how many sheets for 2mm thick,   And would I need to cure this with heat, if so I have a 500 heat platen, 

Thanks guys for any advice,    Kev,   P.s these are for cutting parts on cnc cutter, 