AlessandroPA
AlessandroPA
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 26,
Visits: 301
Thanks a lot. I've started to use the vacuum bagging technique only a few weeks ago and only once I made the bag, not using the appropriate ratio CF-epoxy, but anyway having a good result. With the next bag I would like to have a better balance between the resin and the CF layers, just for this I asked. Thanks
panda (10/05/2015)
ideal would be 50-50 but you need to take into account wastage in the pot, on the brush, in consumables ect so always take this into account when weighing out what you need. Some of the resin will go into the breather when you bag it so will bring it closer to the desired ratio.
Tom
Edited
11 Years Ago by
AlessandroPA
Reply
Like
8
panda
panda
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 47,
Visits: 2.1K
ideal would be 50-50 but you need to take into account wastage in the pot, on the brush, in consumables ect so always take this into account when weighing out what you need. Some of the resin will go into the breather when you bag it so will bring it closer to the desired ratio.
Tom
www.pandakayaks.co.uk
Reply
Like
9
AlessandroPA
AlessandroPA
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 26,
Visits: 301
Ok, thanks. And what about the ratio epoxy resin-carbon fiber, related to the weight of CF? Is it 50-50?
panda (10/05/2015)
If it is epoxy, the exactly as it says on the bottle, any different and you will have problems with it curing and all epoxy resins can be slightly different depending on brand. Polyester then anywhere from 1-5% by volume depending on how fast you want it to gel.
Tom
Reply
Like
9
panda
panda
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 47,
Visits: 2.1K
If it is epoxy, the exactly as it says on the bottle, any different and you will have problems with it curing and all epoxy resins can be slightly different depending on brand. Polyester then anywhere from 1-5% by volume depending on how fast you want it to gel.
Tom
www.pandakayaks.co.uk
Reply
Like
9
AlessandroPA
AlessandroPA
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 26,
Visits: 301
Does anybody know the ratio Component A-Hardener to be used with hand lay up + vacuum bagging technique?
Tags
Hardener
ratio
vacuum bagging
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
10
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search