OKie trying a new part. A pair of the door pulls for my 2006 Lotus Elise.


Here's a pic of the plastic ones in car.

http://carbontuner.com/talk/l1.png


I already installed the plastic ones back in my car so I will have to wait tell I pull the part to show its actual shape. Its a pretty complex part so I am not getting my hopes up on this first run..


http://www.carbontuner.com/talk/l2.png

However this mould is my first "quality" mold. These were the first ones I made since I got the basic mould making technique down.




If Brute Force Isn''''t working your not using enough...
Edited 14 Years Ago by Carbon Tuner
Joe
Joe
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Haha cool stuff, dont forget the pics Wink

 



 


    A $1000 electronic device will always protect a 10 cents fuse
Carbon Tuner
Carbon Tuner
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 104, Visits: 422

Laptop died, got a new laptop, plugged phone into laptop, phone died. It has been an expensive week...

OK well Part came out of the mold good and it was a nice easy cut. I have a dremel 4000 with the easy lock blades; I think it is powerful enough to do most car parts, or maybe a small boat. It has variable speed so it can be adjusted.

Anyhow here’s the part popped out, I use 1x1 twill for the inner 2 layers. This part is ways to complex for that type of weave; I ended up putting more cuts in the fabric of those layers that I would have liked to. Well this is a test part and it has alot of curves making pretty dang stiff for only 3 layers.

Then here's what I need to adjust next time; I keep letting cf clippings get in the surface of my part! Then I need to start positioning the cf on the most visible side. I started on the back where it is facing the glass, I should have started on the side facing inside car. When working with complex parts the weave tends to look better where you started taping/positioning then where you finish.

The Part Un-Cut:

http://carbontuner.com/talk/doorpull2.jpg


The Part Cut:


http://carbontuner.com/talk/doorpull1.jpgNext Run:


Second TRY:

On this run I was sure not to let any pieces fall under the part, I basically did half flipped it up to check under then folder it back down and taped quickly, watching every little snip I took. Also I made the CF fabric much smaller, there’s just no need to have that much excess. What started as a 24” x 16” has been reduced to a 19”x10”. I know it’s hard to see now but when I pull this part you will see the size difference.

http://carbontuner.com/talk/mould.jpg

I am battling 3 small pinholes on the part I cut out, not in the corners or across the whole part, I think it is just 3 tiny air bubbles that surfaced when prepping my part for lacquer. Can I just put wax or black crayon in these? There soo small, really, a pin hole!

http://carbontuner.com/talk/airbubble.jpg


Also will this work as a UV coating or am I throwing this over the hill? My challenge is I bought the spray lacquer, don have an air compressor or gun yet BUT I’m making little parts one at a time, I need lacquer in an aerosol can, this may be it. This is gona suck if I have to fire up the cup gun every time I want to UV protect.


http://carbontuner.com/talk/minwax.jpg

Thanks for reading, please someone help me find aresol UV Laquer, if this is not it.

ONE last question: this laquer, has slightly uneven surface, do I need to apply laquer a bit thicker than paint? Howmany coats would you use? sand inbetween? how do you get your final glow? A compund buff?



If Brute Force Isn''''t working your not using enough...
Edited 14 Years Ago by Carbon Tuner
japcarmaniac
japcarmaniac
Supreme Being (661 reputation)Supreme Being (661 reputation)Supreme Being (661 reputation)Supreme Being (661 reputation)Supreme Being (661 reputation)Supreme Being (661 reputation)Supreme Being (661 reputation)Supreme Being (661 reputation)Supreme Being (661 reputation)
Group: Forum Members
Posts: 53, Visits: 157
im pretty sure most automotive lacquer offers uv protection. upol clear #1 would be a good choice imho if you can get it. 

Edited 14 Years Ago by japcarmaniac
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search