By Carbon Tuner - 1/22/2012 3:20:46 PM
OKie trying a new part. A pair of the door pulls for my 2006 Lotus Elise.
Here's a pic of the plastic ones in car.

I already installed the plastic ones back in my car so I will have to wait tell I pull the part to show its actual shape. Its a pretty complex part so I am not getting my hopes up on this first run..

However this mould is my first "quality" mold. These were the first ones I made since I got the basic mould making technique down.
|