Group: Forum Members
Posts: 433,
Visits: 1.2K
|
I have some prepreg that is close to a year old. I have used it in my AutoClave and it seems to have cured OK. But has it really. Could anyone tell me the signs to look for in prepreg when its no longer good. It didn't seem to be as sticky to the touch as it was when fresh. Any information would be appreciated. Fred
|