Ive seen a few parts with the companies logo in the part (not a sticker on top)

Whats the way of doing this and what material?
Vinly sticker in the mould first, then normal lay up and infuse?
Or put the sticker on the finished part and clear coat over?


kidpaint
kidpaint
Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)
Group: Forum Members
Posts: 99, Visits: 676
Ive heard of people printing the logo out on rice paper then putting it on after the part is made and cleared over like you suggested. I know its been done, but I always question the longevity of vinyl under clear. 
davro
davro
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Hi Darren,

I created an RC body shell out of carbon fibre with stickers.

Once the stickers were applied to the body shell I 2K clear coated the product then sanded flattened back
then applied a few more coats flattened back polished and stickers are hidden in the clear coat.





David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search