By Darren - 3/30/2015 8:24:26 PM

Ive seen a few parts with the companies logo in the part (not a sticker on top)

Whats the way of doing this and what material?
Vinly sticker in the mould first, then normal lay up and infuse?
Or put the sticker on the finished part and clear coat over?

By davro - 3/31/2015 6:16:30 AM

Hi Darren,

I created an RC body shell out of carbon fibre with stickers.

Once the stickers were applied to the body shell I 2K clear coated the product then sanded flattened back
then applied a few more coats flattened back polished and stickers are hidden in the clear coat.