Tapered motocross fork mould??


Author
Message
AlessandroPA
AlessandroPA
Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)
Group: Forum Members
Posts: 26, Visits: 301
I'm making my seatpost for bicycle saddle rolling a CF sheet rolling it around a smaller diameter pipe to reach the wanted diameter

Darren (29/03/2015)
Fasta (28/03/2015)
If you make tube the same size as the smaller end of your forks and then have a single longitudinal cut along it then it should likely snap fit on the tapered fork ok??




Yeah i think thats the way to go, if it doesn't work out i will have to make a tapered plug and mould from that.
Does any one have a link to a thread where they make carbon tube using PVC pipe? I cant seem to find it now

Darren
Darren
Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)
Group: Forum Members
Posts: 54, Visits: 916
Fasta (28/03/2015)
If you make tube the same size as the smaller end of your forks and then have a single longitudinal cut along it then it should likely snap fit on the tapered fork ok??


Yeah i think thats the way to go, if it doesn't work out i will have to make a tapered plug and mould from that.
Does any one have a link to a thread where they make carbon tube using PVC pipe? I cant seem to find it now
VVS
VVS
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Moderators
Posts: 226, Visits: 334
Get some ally bar turned to the same taper and use that as a mandrel.

you could even be clever and have the larger diameter oil seal housing made as a separate bolt on piece and have carbon cover the full length, simply undo it after the resin has set then take the taper out one end and the other piece out the other end.




its possible that the change in diameters could give you problems opening it enough to fit around the fork leg but there's bound to be a work around, flexi resin etc.
redeye
redeye
Supreme Being (686 reputation)Supreme Being (686 reputation)Supreme Being (686 reputation)Supreme Being (686 reputation)Supreme Being (686 reputation)Supreme Being (686 reputation)Supreme Being (686 reputation)Supreme Being (686 reputation)Supreme Being (686 reputation)
Group: Forum Members
Posts: 52, Visits: 559
I'm not sure what bike you have there, but I love the triple clamps, look awesome. Agreed that a vertical slit would be the way to go. I will also add that they should be stuck on so as not to rattle and cause damage to your fork tubes. Something that will be thin and isolate the fork protectors from the fork tubes would be wise, I'd recommend silicon adhesive that is non acidic as this will eat into the aluminum. If you're not fond of having a the slit opened larger at the top due to the taper then perhaps best to make a tapered mold/plug by machining something on a lathe - some hardwood that could be coated for a better finish perhaps. Just an idea. Will be great to see how these come along, I'll probably make some for my bike. 
Fasta
Fasta
Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
If you make tube the same size as the smaller end of your forks and then have a single longitudinal cut along it then it should likely snap fit on the tapered fork ok??




Darren
Darren
Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)
Group: Forum Members
Posts: 54, Visits: 916
Im looking to make some fork covers/protectors like in the image below but my forks have a slight taper on them.
I was thinking on using the pvc pipe trick to make some carbon tubes but I'm not sure how well they would fit on a tapered fork.
Any ideas on what i can do?


Thanks 








GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search