I'm making my seatpost for bicycle saddle rolling a CF sheet rolling it around a smaller diameter pipe to reach the wanted diameter
Darren (29/03/2015)
Fasta (28/03/2015)
If you make tube the same size as the smaller end of your forks and then have a single longitudinal cut along it then it should likely snap fit on the tapered fork ok??Yeah i think thats the way to go, if it doesn't work out i will have to make a tapered plug and mould from that.
Does any one have a link to a thread where they make carbon tube using PVC pipe? I cant seem to find it now