I always keep cores away from the edges of laminates anyway. So leave the core about 2" short of the edges, and build up the thickness using strips of cloth or woven tape. 
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
You could place one layer of black Diolen between  your first layer of carbon and the cormat and this will keep the cost down.
Chris
Carbon fibre works LTD 

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
When you say fussy it depends in how fussy.

you could simply use paint or there's the black repair resin.

if the edges are straight you could go the full hog and get thin carbon strips water jet cut and glued on or possibly work the carbon around the core.




ive never used core materials so some pf the seasoned guys may have a definite way to work.
Dcg
Dcg
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Forum Members
Posts: 1, Visits: 11
hi, I am new to carbon, looking to make a set of carbon panels for a customers car. Due to the size of the panels I was planning on having 1 layer of carbon, 3mm Lantor Coremat, 1 layer of carbon. My problem is that the Lantor Coremat is white and the carbon is black, there are a few panels where you'll be looking at it edge on so will see the White Lantor Coremat. What's the best way to colour the Coremat black? My customer is fussy and I know they won't be happy seeing White Coremat. Is the best way to lay up the first layer of carbon allow to start curing then apply the Coremat with black pigment in the resin, again allow to start curing before adding the final layer of carbon.

Thanks in advanced!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search