Easy Composites Team,

I recently purchased a sheet of rigid CFRP and need to model the material using LS Dyna.
I am using the material model 162 and require the following properties;
density
Young’s modulus - longitudinal direction 
Young’s modulus - transverse direction 
Young’s modulus - through thickness direction
Poisson’s ratio ba
Poisson’s ratio ca 
Poisson’s ratio cb 
shear modulus ab 
shear modulus bc 
shear modulus ca
Longitudinal tensile strength 
Longitudinal compressive strength  
Transverse tensile strength 
Transverse compressive strength 
Through thickness tensile strength 
Crush strength 
Fiber mode shear strength 
Matrix mode shear strength
Matrix mode shear strength
Matrix mode shear strength

I am aware that some of these values will be the same and some can be calculated from others however as much information you have as possible would be great thanks.

Regards.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search