Hi, I am trying to preserve some delicate model aircraft kits my father assembled and my idea is to encapsulate them in a clear setting material that will not damage them in the process. Can anyone help guide me ?
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
It depends on the plastics and the finishing paints/decals.  Most plastics would be fine with our Waterclear Polyurethane Casting Resin however you would need to test it on the paints/decals to ensure the finish isn't ruined.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant