Encapsulating plastic model aircraft in clear material
Encapsulating plastic model aircraft in clear material
Post Reply
Like
3
Encapsulating plastic model aircraft in clear material
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
dhamer
dhamer
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 6
Hi, I am trying to preserve some delicate model aircraft kits my father assembled and my idea is to encapsulate them in a clear setting material that will not damage them in the process. Can anyone help guide me ?
Tags
Encapsulation
Reply
Like
3
Warren (Staff)
Warren (Staff)
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8K
It depends on the plastics and the finishing paints/decals. Most plastics would be fine with our
Waterclear Polyurethane Casting Resin
however you would need to test it on the paints/decals to ensure the finish isn't ruined.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search