Hello,




We have been attempting to infuse carbon fiber fabric with some custom made vinyl ester resin visc aroung 400. We are all new to this so any advice would be appreciated.

The equip we r using for the infusion is:

-Vacuum pump 2.5cfm

-resin trap with gauge (paint sprayer can) 

-bagging - http://www.fibreglast.com/product/stretchlon-200-bagging-film-1678/Vacuum_Bagging_Films_Peel_Ply_Tapes

-release film perforated - http://www.fibreglast.com/product/low-temperature-release-film-1580/Vacuum_Bagging_Films_Peel_Ply_Tapes

-flow media - http://www.fibreglast.com/product/HDPE_Flow_Media_1406/Vacuum_Bagging_Vacuum_Infusion

We are getting a consistent seal, no leaks pretty much every time we attempt. But we still get small pitting or pin holes consistently thru out the carbon fiber.




Thanks,

Don












GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search