Post Curing Uni-Mould System


Author
Message
ECV3
ECV3
Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)
Group: Forum Members
Posts: 30, Visits: 106
Can anyone give me advice on post curing uni-mould system moulds for use with low to mid temp pre preg. On EC's pdf it says-

10hrs at 60c >  2hrs at 70c >  2hrs at 80c >  2hrs at 90c

My question is are times and temps correct and do i need to use specific Ramp Rates?

Cheers!