Can anyone give me advice on post curing uni-mould system moulds for use with low to mid temp pre preg. On EC's pdf it says-
10hrs at 60c > 2hrs at 70c > 2hrs at 80c > 2hrs at 90c
My question is are times and temps correct and do i need to use specific Ramp Rates?