Hi all,
I'd like to show you a quick video about my split board for kitesurfing.

From a composites point of view  the board was obtained by an infusion process in the bottom and a lamination on the top.
In the bottom I also tryed to mix spread tow carbon fabric with aluminized glass in order to obtain something different from a graphical point of view.

The board core is balsa wood.

The video     https://www.youtube.com/watch?v=RoHH2grML8U


And some pictures

http://i38.servimg.com/u/f38/13/17/52/45/710.jpg

http://i38.servimg.com/u/f38/13/17/52/45/210.jpg

http://i38.servimg.com/u/f38/13/17/52/45/1610.jpg

http://i38.servimg.com/u/f38/13/17/52/45/910.jpg

http://i38.servimg.com/u/f38/13/17/52/45/810.jpg

http://i38.servimg.com/u/f38/13/17/52/45/1110.jpg

http://i38.servimg.com/u/f38/13/17/52/45/211.jpg

http://i38.servimg.com/u/f38/13/17/52/45/310.jpg

http://i38.servimg.com/u/f38/13/17/52/45/miniat10.jpg





My You Tube Channel
Tags
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search