Hi all,
I'd like to show you a quick video about my split board for kitesurfing.

From a composites point of view  the board was obtained by an infusion process in the bottom and a lamination on the top.
In the bottom I also tryed to mix spread tow carbon fabric with aluminized glass in order to obtain something different from a graphical point of view.

The board core is balsa wood.

The video     https://www.youtube.com/watch?v=RoHH2grML8U


And some pictures

http://i38.servimg.com/u/f38/13/17/52/45/710.jpg

http://i38.servimg.com/u/f38/13/17/52/45/210.jpg

http://i38.servimg.com/u/f38/13/17/52/45/1610.jpg

http://i38.servimg.com/u/f38/13/17/52/45/910.jpg

http://i38.servimg.com/u/f38/13/17/52/45/810.jpg

http://i38.servimg.com/u/f38/13/17/52/45/1110.jpg

http://i38.servimg.com/u/f38/13/17/52/45/211.jpg

http://i38.servimg.com/u/f38/13/17/52/45/310.jpg

http://i38.servimg.com/u/f38/13/17/52/45/miniat10.jpg





My You Tube Channel
Tags
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Very impressive Bruce and a very professional video of your work !



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Edited 11 Years Ago by davro
Brian_s
Brian_s
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Very nice. Well done.

Brian.
VVS
VVS
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Very impressed.
Real nice work and love the quality of the video.
Watched your hydrofoil board video and that is sick man, just looks so wrong and yet so right sat out of the water. 