Bazz
Bazz
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 16
Having trouble holding vacuum! Have checked from the bag to the catch pot to the pump holding vacuum here. Installed a new bag even ran a dye around the edge, inlets/outlets and pleats no leaks. which only leaves the mold, this is made from 18mm custom wood with glued joints and 5 layers of epoxy paint hard to see it leaking. do you have any ideas? Could I infuse it and leave the pump running? Help Regards. 
GO