Talk Composites - The Forum for Advanced Composites

Holding Vacuum

http://www.talkcomposites.com/Topic15242.aspx

By Bazz - 2/24/2015 10:52:50 PM

Having trouble holding vacuum! Have checked from the bag to the catch pot to the pump holding vacuum here. Installed a new bag even ran a dye around the edge, inlets/outlets and pleats no leaks. which only leaves the mold, this is made from 18mm custom wood with glued joints and 5 layers of epoxy paint hard to see it leaking. do you have any ideas? Could I infuse it and leave the pump running? Help Regards. 
By Warren (Staff) - 2/26/2015 9:05:56 AM

No problem. Just make sure the worktable is clean and free of sharp objects and the back side and edges of the mould have no sharp edges that could puncture the bag and you should be fine.