Went back to drawing board and came up with some extra flanges.
Do i need to block up the holes underneath ?.
Next job DIY catch tank for resin infusion any ideas ?
http://i230.photobucket.com/albums/ee247/boustie/IMAG1569.jpg
Warren
Warren
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Administrators
Posts: 214, Visits: 782
not heard of anyone trying it that way.  Youd realistically need a flat surface to stabilise the bagging stack, eg if its flatish part you could lay it on some polyprolene sheet. Youd have to lightly glue it down, and seal the holes and edges with wax, but it should give you a solid enough surface to do a one off part without making a full mould. If theres a big curve, the air under the part could be an issue as the wax in one place will pull out as the vacuum draws to draw air out under the part.

You could of course make temporary flanges on the part and envelope bag the whole thing to give you the rigidish edges you want to give a clean edge line.
boustie
boustie
Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)
Group: Forum Members
Posts: 18, Visits: 92
I think what im trying to say is because i dont have a mould with an area around the mould to fix the bagging stack to, will the resin flow ok through the material. ? 
boustie
boustie
Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)
Group: Forum Members
Posts: 18, Visits: 92
I want to try resin infusion on this.

I plan to the cut and lay the bagging stack slightly bigger then the part.

The part will be sat on top of the bagging film

Will this be ok 

advise appreciated.

http://i230.photobucket.com/albums/ee247/boustie/IMAG1552.jpg