I want to try resin infusion on this.

I plan to the cut and lay the bagging stack slightly bigger then the part.

The part will be sat on top of the bagging film

Will this be ok 

advise appreciated.

http://i230.photobucket.com/albums/ee247/boustie/IMAG1552.jpg
By boustie - 5/3/2012 10:57:25 AM

Went back to drawing board and came up with some extra flanges.
Do i need to block up the holes underneath ?.
Next job DIY catch tank for resin infusion any ideas ?