As a general rule, double the weight of the cloth to get the weight of fibre and resin
JLakoda
JLakoda
Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)
Group: Forum Members
Posts: 1, Visits: 3
I can find the weight of carbon fiber cloth, but how much does it weigh after resin is applied?
Specifically what I'd like to know is how much a square meter would weigh if there were two layers of .25 mm fabric plus the necessary resin?