I can find the weight of carbon fiber cloth, but how much does it weigh after resin is applied?
Specifically what I'd like to know is how much a square meter would weigh if there were two layers of .25 mm fabric plus the necessary resin?
By ajb100
-
1/30/2015 9:24:07 AM
As a general rule, double the weight of the cloth to get the weight of fibre and resin