Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
tips on using soric for the first time
tips on using soric for the first time
Post Reply
Like
3
tips on using soric for the first time
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Jdmleesy
Jdmleesy
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 39,
Visits: 380
Hi all
Iv been making smaller parts using infusion the EC way with some nice finishes so i want to have a go at making a bonnet
Im going to make it the same as the vid on the site using
200g carbon
2mm soric
200g carbon
Has anybody got any tips on using the soric because iv never used it b4 and im worried about print thru and i want it to go well first time
And any tips or advice on doing bigger parts in general?
Does it normally take longer to infuse use soric?
Ne help is much appreciated
Thanks daz
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
tips on using soric for the first time
Jdmleesy
-
10 Years Ago
I've started using it recently and it is extremely easy to use! Treat it just like cloth and you'll...
FLD
-
10 Years Ago
Flow speed will depend on your resin system and other factors so it's difficult to give guidance...
Hanaldo
-
10 Years Ago
Ok cheers lads Do u think it would be best to use just the slow hardener to prevent gelling up...
Jdmleesy
-
10 Years Ago
The bonnet is roughly a metre sq
Jdmleesy
-
10 Years Ago
Print-through is a phenomenonthat will always occur to some extent. You can do things to reduce it...
Warren (Staff)
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search