Correct Adhesive for CF Tube and Nylon


Author
Message
shuriken1
shuriken1
Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)
Group: Forum Members
Posts: 2, Visits: 7
Hi,

I intend to glue some of your 22.2mm ID CF Tube to a 3d printed part which I've been told is PA-2200 (Nylon). Going by your website, the PT326 adhesive seems most appropriate for the job. Can anyone please confirm whether that's correct and if not, which adhesive is best?

Thanks very much,

Sam.
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Bonding to nylons is always difficult due to the low reactivity surface.

The glue I would recommend is our VuduGlu™ VM100 Black.

For best results you will need to key both surfaces and with the nylon use flame treatment to increase the reactivity of the surface.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
shuriken1
shuriken1
Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)
Group: Forum Members
Posts: 2, Visits: 7
Ok, thanks Warren. I'll make sure I get that stuff.

All the best.