Looking real good Andy, I would imagine there is a good weight saving compared with the original seats!

Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
+1 ^

I'd be in trouble there. I'm flinching just thinking about it. 
ajb100
ajb100
Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Looking good

My wife would be no where near as accommodating!
andygtt
andygtt
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
Thought I would do a quick update, made the other seat and changed the upulstery a little, was in a rush to get it ready for the Autosport show so they still need lacquering and some refinement to the upulstery but am pretty happy with the end result.








davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Nice job on developing your own buck it sure looks nice.
Think you might have convinced me that making my own seat buck suited for myself and the car is the best course for my project.

Thanks for sharing those pdf's Warren very interesting read.

The idea of making resin infused carbon fibre wheels put a childish smile on my face.



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Edited 11 Years Ago by davro
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Pre-preg made parts aren't necessarily superior to well made infused parts, but in terms of layup, the tacky nature and pre-measured resin nature of pre-preg makes it better suited to wheels in that case as it just makes life easier.

This article was a paper by one student of an FSAE team doing carbon wheels:

https://kb.osu.edu/dspace/bitstream/handle/1811/58422/carbon_wheel_thesis_FINAL.pdf?sequence=1

Well worth a read.  Also plenty of threads on FSAE forums.

Another good read:
http://seit.unsw.adfa.edu.au/ojs/index.php/juer/article/viewFile/450/278

you can get kevlar pre-pregs but usually such things are mostly used in fairly specialist applications so made to contract and unlikely to be something that can be easily got in small amounts.

It was a busy weekend! Just ring if you need to catch up or ask stuff.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
andygtt
andygtt
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
Hi Warren
Sorry we didn't have a proper catchup at Autosport, wanted to have a proper chat... was a bit mad the entire weekend.

Do you have details or links to these wheels the formula students do? or do they keep it under wraps?

I keep thinking a wheel along the lines of the dymag car rims with a machined alloy centre (machine down a normal road rim) and a carbon rim.... I should be able to make a very stiff rim... 

Not sold on pre prey being superior... I would like to add differing reinforcements such as Kevlar, is that available in pre preg?
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
In terms of wheels, almost anything is possible with enough forthought but its likely to be very very difficult.  Nothing to say you cant in theory infuse a rim shape. However youve got to get the fabric to stay where it is, and ideally you don't want excessive spray tack usage in structural parts. Then the nature of infusion means it may not be perfectly even all the way round making balancing an issue.

Pre-pregs would be much more consistant and infinitely easier to lay up. 

All the formula student ones I've seen used pre-pregs.  Some used multiple parts bonded together, others devised a more complicated one piece approach.  Some went for carbon rims and billet machined alloy centres.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
andygtt
andygtt
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
Seat is my own Shape, taken me around a year to develop the buck Smile
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Looks really nice andygtt like the leather work Cool
 
Out of interest what seat is it based on ?

Carbon fibre car wheel would it even be possible with resin infusion ...



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Edited 11 Years Ago by davro
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search