hello, i am engaged in a different kind of project; i am trying to create cast picture frames for my artwork. i like the look of silicone and rubber, and epoxy and i want to embrace these materials and leave them unpainted in their raw form. 

I am new to casting. I would greatly appreciate advice on which methods and materials to use to create "perfect" picture frames. I want them to look like they came out of a factory.  I have a small but diverse range of tools at my disposal. 


I have attached here my first master ("pattern") and a wooden contain to pour mould materials into.  I bought some epoxy resin at a boat supply store and I am thinking it will work to create a mould. I have some beeswax to use as a release agent. 

I have two general questions:

Will my method work well?

What is the best method of system make by easy composites that I would use to make the best moulds and castings possible? 

I am concerned that this method will not work because the frame is so thin and all the sides are parallel. I don't really know how i will possibly get a casting out of the mould. Any ideas here are welcome too. the frame made of acrylic, show in the photo, is about 12x16x3cm. it has a lip on the top of it to hold the glass pane in place.

Hope to hear from someone. Thanks!
Edited 11 Years Ago by Michael77
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search