Helicoils or what? How do i inser it? Help please :)


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
ultimately there are loads of different methods you can use.

You have to bear in mind that composites generally will not take a thread and generally do not like point loading forces.

With that in mind, items like bighead fasteners are ideal as they solve both issues, however repair washers, home made bigheads etc can be equally as effective.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Watch the EC bonnet making tutorial on the Tube ... part three deals with bonding on fasteners ...
I normally use home made ones.. I have a friend who Tig welds stainless bolt studs to small plates made from 1 - 2 mm stainless steel sheet

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Edited 11 Years Ago by Dravis
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Cannot stand riv nuts. For composites, always something along the lines of big head bonding fasteners. It's easy to make your own if you're on a budget
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
So you've made a bonnet? How does the factory one attach? If it needs a threaded insert, I would use a nutsert or a rivnut. 
migor
migor
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Forum Members
Posts: 1, Visits: 7
Hi!
I bought some carbon fiber and made my mould and so on.
But i could not see now when I got to the problem. That how do
I insert helicoils or some thing like it to be able to get the hood onto my car?
Without cracking the part or making the metal start to corrosion.

Sorry for my bad english.

Thanks for your help! Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search