Group: Forum Members
Posts: 468,
Visits: 2.7K
|
If it helps I stuck with vac bagging for a loooong time. I didn't see the point of infusion when I could make perfectly adequate parts with a bag. I tried it and now I would infuse through choice. It is that good!
|